Technical guidance and specification product covering laminated glass delamination causes,prevention,and edge defect remediation. Addresses common failure modes including PVB edge moisture absorption,autoclave under-cure,incompatible sealants,and improper edge protection. Our production team provides consulting on lamination quality expectations,edge defect acceptance criteria,and specification of lamination type appropriate for environmental exposure conditions. Essential technical resource for architects,glazing contractors,and building envelope consultants specifying laminated glass for outdoor applications,exposed edges,and point-fixed glazing systems.
Delamination of Laminated Glass and Edge Defects represent the primary failure modes affecting laminated glass performance and longevity. Understanding the causes and prevention of these issues is essential for proper product specification and quality assurance. Delamination occurs when the bond between the interlayer and glass fails,creating visible cloudy or opaque areas that progress from the edge inward. The most common cause of PVB delamination is moisture absorption at exposed edges. PVB is hygroscopic,meaning it absorbs moisture from the atmosphere,which plasticizes the interlayer and reduces adhesion strength. When glass edges are directly exposed to rain,condensation,or high humidity without adequate edge protection,moisture wicks into the PVB causing progressive delamination that appears as a milky white band advancing from the edge. This is why PVB laminated glass should not be used with exposed edges,at cutouts,or in high-humidity environments unless specifically designed edge protection measures are incorporated into the glazing system design.
Edge defects in laminated glass take several forms beyond moisture-related delamination. Bubbles near edges can result from insufficient autoclave pressure or temperature,entrapped air that was not removed during pre-press processing,or residual volatiles from dirty glass surfaces. Incorrect interlayer positioning that leaves the PVB edge flush with or extending beyond the glass edge creates a path for accelerated moisture and chemical attack. Chemical incompatibility between PVB and certain sealant types,particularly acidic cure silicones or oil-based glazing compounds,can cause localized interlayer degradation at the edge-sealant interface. Heat-related edge defects including edge blisters can occur when laminated glass is processed through tempering furnaces for heat-strengthening,as the localized heating at edges can volatilize moisture trapped in the interlayer. Understanding these failure mechanisms allows proper product selection and detailing at the design stage to prevent costly field failures.
Proper specification and detailing are the most effective measures against delamination. For applications with exposed edges,EVA or SGP interlayers should be specified as they are inherently moisture-resistant and do not suffer PVB delamination failure modes. For PVB laminated glass with exposed edges,edge sealing with compatible polysulfide or neutral-cure silicone sealants provides temporary protection but should not be relied upon as a permanent solution over the building lifespan. Our technical team provides consulting on lamination type selection,edge condition detailing,sealant compatibility,and quality assurance testing including boil testing per EN ISO 12543-4 to verify lamination quality. We also offer factory edge sealing services with UV-stable sealants for applications where full edge coverage in the glazing system cannot be guaranteed.