Structural glazing insulated glass units with two-part structural silicone secondary seal engineered for structurally glazed,two-side SSG,and four-side SSG curtain wall systems. Our structural silicone IGUs are tested per ASTM C1135 for tensile adhesion and ASTM C1184 for structural performance,with design strength values verified through project-specific adhesion testing. The structural silicone bond transfers wind load and glass dead load from the glass to the supporting frame,eliminating the need for mechanical retainers. Available in all standard IGU configurations with full structural calculation support and project-specific test reports.
Structural Glazing IGU with silicone secondary seal is the specialized IGU product required for structurally glazed curtain wall systems where the glass is adhered directly to the supporting aluminum frame using structural silicone,with no external mechanical pressure plates or caps. In this system,the structural silicone bead applied to the IGU perimeter bonds to both the IGU surface and the aluminum frame,creating the structural connection that supports the glass dead load (weight) and transfers wind loads to the building structure. The secondary sealant on the IGU itself must be a compatible silicone formulation because silicone bonds only to silicone: applying structural silicone to a non-silicone secondary seal (such as polysulfide or polyurethane) creates a weak bond interface that will fail under structural loads. Therefore,all IGUs intended for structural glazing applications must be manufactured with a two-part neutral-cure structural silicone as the secondary seal,compatible with the field-applied structural silicone used by the curtain wall contractor.
The structural performance of silicone-sealed IGUs is verified through a rigorous testing and engineering process defined by ASTM C1401 (Standard Guide for Structural Sealant Glazing). The IGU manufacturer must provide tensile adhesion test data for the specific glass-coating-silicone combination per ASTM C1135,demonstrating adequate adhesion strength and cohesive failure mode. The design strength of the structural silicone,typically 20 psi (138 kPa),is applied to the calculated bite (sealant contact width) to verify that the sealant can support the design loads with appropriate safety factors. Project-specific adhesion testing is normally required by specification,where samples of the actual glass (including any coatings at the bond surface),the actual silicone,and the actual aluminum finish are assembled and tested per ASTM C1135. For SSG IGUs,this testing must verify adhesion of the structural silicone to both the IGU secondary seal and the aluminum frame coating.
Our structural glazing IGU production uses dedicated two-part silicone mixing and dispensing equipment with precise ratio control and continuous bead integrity monitoring. The IGU secondary seal is a neutral-cure two-part structural silicone with tensile strength exceeding 345 kPa and elongation exceeding 200 percent per ASTM C1135. Standard configurations include all Low-E,tinted,reflective,and spandrel glass options,with the structural silicone bond surface carefully specified to avoid coating delamination or adhesion interference. We maintain a comprehensive library of adhesion test data for common glass coating,silicone,and aluminum finish combinations. For each project,we provide structural silicone design calculations,recommended bite dimensions,project-specific adhesion test coordination,and IGU certification documentation. Our engineering team coordinates with curtain wall system manufacturers and structural engineers to ensure the SSG IGU specification is fully integrated with the framing system design and structural calculations for building permit approval.